PENGARUH FAKTOR AIR SEMEN (FAS) DAN MIX DESIGN PADA PEMBUATAN BATA BETON (PAVING BLOCK) TERHADAP KUAT TEKAN
ARIEF WAHYULIE, Ir. Bambang Herumanta. MT
2014 | Skripsi | D3 TEKNIK SIPILPaving block banyak digunakan dalam bidang konstruksi, seperti pavement, jalan raya, lahan parkir. Kemudahan dalam pemasangan, perawatan yang murah serta memenuhi aspek keindahan mengakibatkan paving block lebih banyak disukai. Pembuatan paving block belum optimal dari sisi kualitas, karena masih dibuat dalam skala kecil sebagai produk home industri. Kekuatan paving block akan diuji pada beberapa paving yang dibuat dengan metode pemadatan penuh, pemadatan bertahap, serta digetarkan. Penelitian dilaksanakan di Laboratorium bahan bangunan Program Diploma teknik sipil SV UGM. Dibuat 5 (lima) variasi komposisi paving block yang terdiri dari Semen, Pasir, yaitu 1:3, 1:4, 1:5, 1:6, 1:7. Setiap variasi dibuat dengan faktor air semen (0.40, 0.45, 0.50, 0.55, 0.60) dengan total benda uji 125 paving (setiap variasi dibuat 5 benda uji). Perawatan dilakukan dengan menyiram permukaan paving sampai umur 7, 14, dan 21 hari. Dari hasil pengujian rata-rata diperoleh dengan faktor air semen 0.40 dengan kuat tekan 2.103 Mpa, 0.45 dengan kuat tekan 2.589 Mpa, 0.50 dengan kuat tekan 2.939 Mpa, 0.55 dengan kuat tekan 3.574 Mpa, 0.60 dengan kuat tekan 4.092 Mpa.
Paving block most use in construction such as pavement, highway and parking area. Ease on setting, cheap of treatment and aesthetic fully cause of paving block such as like. Production of paving block is not optimally from quality, because paving block still from the home industry product. The strength paving block testing at some paving product with full-pressing method, partial-pressing method and vibrating method. The research was done in CV UGM civil technique diploma labotary. The five series paving block consist of cement : sand are 1:3, 1:4, 1:5, 1:6, 1:7 respectively. Each variant was made with water cement ratio ( 0.40, 0.45, 0.50, 0.55, 0.60 ) with totally specimen are 125 (each series was made 5 specimen). Curing method is done with spray water surface on paving block of age ; 7, 14, and 21 days, respectively. From result of examination of mean obtained water cementy ratio 0,40 with compresive strength 2.103 Mpa, 0.45 with compresive strength 2.589 Mpa, 0.50 with compresive strength 2.939 Mpa, 0.55 with compresive strength 3.574 Mpa, 0.60 with compresive strength 4.92 Mpa.
Kata Kunci : -