Laporkan Masalah

Studi Kinetika Pemulihan Tellurium dari Copper Anode Slime (CAS) Menggunakan Electrowinning

Maria Kristiani, Prof. Himawan Tri Bayu Murti Petrus, S.T., M.E., D.Eng. ; Ir. Sutijan, M.T., Ph.D.

2026 | Tesis | S2 Teknik Kimia

Tellurium (Te) merupakan salah satu unsur kritis yang banyak digunakan dalam industri strategis, terutama pada teknologi fotovoltaik, termoelektrik, dan material semikonduktor. Sumber utama tellurium umumnya berasal dari copper anode slime (CAS), yaitu limbah hasil pemurnian tembaga yang masih mengandung unsur bernilai. Oleh karena itu, pemulihan tellurium dari CAS penting dilakukan untuk meningkatkan nilai tambah limbah industri tembaga dan mendukung ketersediaan mineral kritis. Penelitian ini bertujuan untuk menganalisis pengaruh suhu dan densitas arus terhadap pemulihan serta kemurnian tellurium, serta mengevaluasi model kinetika yang merepresentasikan laju penurunan konsentrasi tellurium dalam larutan selama proses electrowinning. Pada penelitian ini, CAS terlebih dahulu diproses melalui tahap pelindian dalam media NaOH untuk menghasilkan larutan yang mengandung spesies tellurium terlarut. Selanjutnya, proses electrowinning dilakukan secara galvanostatik menggunakan katoda stainless steel, anoda titanium berlapis platina, dan elektroda referensi Hg/HgO. Variasi suhu yang digunakan adalah 25, 50, dan 70 °C, sedangkan variasi densitas arus adalah 100, 160, dan 200 A/m². Konsentrasi tellurium dalam larutan dianalisis menggunakan ICP-OES, sedangkan deposit hasil electrowinning dikarakterisasi menggunakan SEM-EDX. Hasil penelitian menunjukkan bahwa peningkatan suhu menghasilkan recovery dan kemurnian Te yang lebih tinggi. Densitas arus menunjukkan kondisi optimum pada nilai tengah, yaitu 160 A/m². Kondisi terbaik diperoleh pada suhu 70 °C dan densitas arus 160 A/m², dengan recovery Te sebesar 94,65?n kemurnian deposit Te sebesar 78,44%. Efisiensi arus tertinggi diperoleh pada suhu 70 °C dan densitas arus 100 A/m², yaitu 41,47%, sedangkan konsumsi energi spesifik berada pada rentang 3,19–6,76 kWh/kg Te. Hasil SEM-EDX menunjukkan bahwa deposit berbentuk agregat partikel tidak beraturan dengan permukaan kasar, dan kandungan Te terdeteksi sebesar 80,00 wt%. Evaluasi kinetika dengan model pseudo-first-order menghasilkan nilai kobs sebesar 0,0051–0,0174 menit?¹ dan nilai R² sebesar 0,8703–0,9853. Model empiris dengan komponen kuadratik densitas arus memberikan hasil terbaik, dengan R² validasi 0,9302, SSE 1,26 × 10??, energi aktivasi 17,35 kJ/mol, dan densitas arus optimum 161,74 A/m².

Tellurium (Te) is a critical element widely used in strategic industries, particularly in photovoltaic technology, thermoelectric materials, and semiconductor applications. Tellurium is commonly recovered from copper anode slime (CAS), a by-product of copper refining that still contains valuable elements. Therefore, recovering tellurium from CAS is important for increasing the added value of copper industry waste and supporting the availability of critical minerals. This study aimed to investigate the effects of temperature and current density on tellurium recovery and deposit purity, as well as to evaluate a kinetic model representing the decrease in tellurium concentration in the electrolyte during the electrowinning process. CAS was initially leached in NaOH medium to produce a solution containing dissolved tellurium species. The electrowinning process was subsequently conducted under galvanostatic conditions using a stainless-steel cathode, a platinum-coated titanium anode, and an Hg/HgO reference electrode. The temperatures investigated were 25, 50, and 70 °C, while the current densities were 100, 160, and 200 A/m². The tellurium concentration in the electrolyte was analyzed using ICP-OES, while the resulting deposits were characterized using SEM-EDX. The results showed that increasing the temperature enhanced both Te recovery and deposit purity. An optimum response to current density was observed at the intermediate value of 160 A/m². The best operating condition was obtained at 70 °C and 160 A/m², resulting in a Te recovery of 94.65% and a deposit purity of 78.44%. The highest current efficiency of 41.47% was obtained at 70 °C and 100 A/m², while the specific energy consumption ranged from 3.19 to 6.76 kWh/kg Te. SEM-EDX analysis showed that the deposit consisted of irregular particle aggregates with a rough surface, with a detected Te content of 80.00 wt%. Kinetic evaluation using the pseudo-first-order model yielded k_obsvalues of 0.0051–0.0174 min?¹ and R² values of 0.8703–0.9853. The empirical model incorporating a quadratic current-density term provided the best performance, with a validation R² of 0.9302, an SSE of 1.26 × 10??, an apparent activation energy of 17.35 kJ/mol, and an optimum current density of 161.74 A/m²

Kata Kunci : copper anode slime, electrowinning, kinetika, NaOH, tellurium

  1. S2-2026-540851-abstract.pdf  
  2. S2-2026-540851-bibliography.pdf  
  3. S2-2026-540851-tableofcontent.pdf  
  4. S2-2026-540851-title.pdf